Extent:
1 Online-Ressource (27 p.)
Illustrationen (farbig)
Type of publication: Book / Working Paper
Language: English
Notes:
Bibl. : p. 25-26
ISBN: 978-92-79-22607-6
Other identifiers:
10.2790/40313 [DOI]
Source:
ECONIS - Online Catalogue of the ZBW