Selective Oxidation and Internal Nitridation of Singlecrystalline Nickel-Base Superalloys
Year of publication: |
1998
|
---|---|
Authors: | Chang, S.Y. ; Krupp, U. ; Christ, H.-J. |
Published in: |
Metall : Fachzeitschrift für Metallurgie ; Technik, Wissenschaft, Wirtschaft. - Clausthal-Zellerfeld : GDMB-Informationsges, ISSN 0026-0746, ZDB-ID 2077589. - Vol. 52.1998, 6, p. 355-359
|